Low-density PE and FP as matrixes and MWCNTs and grinded EG as fillers were chosen for preparation of NCM samples for testing.A special vacuum mold with a spinner was used to make the samples by extruding the NCM molten mixture. Parameters of nanotubes were as follows: average diameter of 10-20 nm, specific surface area (determined by argon desorption method) of 200-400 m2/g, and poured bulk density varying from 20 to 40 g/dm3.Polyethylene and carbon nanotubes-based powder mixtures were mechanically milled in a drum mixer.Low-density PE is a moisture- and corrosion-resistant and price-accessible raw material.